Titanium 6Al-6V-2Sn is a two-phase, Alpha Beta Alloy. It is usually used in the annealed or solution treated and aged conditions. It’s a heat treatable, high strength alloy with lower toughness and ductility than Titanium Grade 5 (6Al-4V) and it’s difficult to weld. Cold forming of Titanium 6Al-6V-2Sn is difficult because of its high strength and the large amount of spring-back that results. This grade can be welded by the inert gas shielded, fusion welding process but the heat effected area will have less ductility and toughness than the parent material. The hardness of Titanium 6-6-2 is approximately Rockwell C 36-38. This grade is primarily used for airframe and jet engine parts, rocket engine cases and ordinance components. Please call us to determine our minimum item quantity.
C | N | O | H | Si | Mo | V | Al | Fe | Sn | Zr |
---|---|---|---|---|---|---|---|---|---|---|
.08 max | .05 max | .12 max | .010 - .125 | .10 max | 1.75 - 2.25 | 3.5 - 4.5 | 5.5 - 6.5 | .25 max | 1.75 - 2.25 | 3.5 - 4.5 |